Molecular Formula | C3H3N3S3 |
Molar Mass | 177.27 |
Density | 1.589 (estimate) |
Melting Point | >300 °C (lit.) |
Boling Point | 242.5±23.0 °C(Predicted) |
Flash Point | 207.268°C |
Water Solubility | Slightly soluble in water. |
Vapor Presure | 0Pa at 25℃ |
Appearance | Yellow amorphous powder |
Color | Yellow |
pKa | 6.35±0.20(Predicted) |
Storage Condition | Inert atmosphere,Room Temperature |
Refractive Index | 1.5800 (estimate) |
MDL | MFCD00006052 |
Physical and Chemical Properties | Melting point> 300°C |
Hazard Symbols | Xi - Irritant |
Risk Codes | 36/37/38 - Irritating to eyes, respiratory system and skin. |
Safety Description | S24/25 - Avoid contact with skin and eyes. S36 - Wear suitable protective clothing. S26 - In case of contact with eyes, rinse immediately with plenty of water and seek medical advice. |
WGK Germany | 2 |
RTECS | XZ2830000 |
TSCA | Yes |
HS Code | 29309090 |
Hazard Note | Irritant |
LogP | 0.73 at 25℃ |
EPA chemical substance information | information provided by: ofmpeb.epa.gov (external link) |
purpose | This product is a crosslinking agent for halogen-containing polymers. Its anti-aging properties can be used in Diene Rubber, and has adhesion, can be polymer and metal adhesion, is also a kind of copper damage inhibitor. 2,4, 6-trimercapto-1, 3, 5-triazine compounds are widely used as heat stabilizers for polypropylene, rubber and other polymers, chlorinated ethyl acrylate-Ethylene polymers, curing Agent of acrylic rubber and other polymers, suitable for acrylate rubber ACM, chloro ether Rubber CO.ECO and chloroprene rubber CR, can also be used for rubber and plastic blend materials, this product is fast vulcanization speed, scorch safety, can shorten the vulcanization time, without two stage vulcanization, made of vulcanized rubber oil resistance, heat-resistant and pressure-resisting remarkable vulcanizate has good mechanical properties. It is a special vulcanizing agent for acrylate rubber. As a special vulcanizing agent, it can also be used for chlorohydrin rubber and chloroprene rubber, and can also be used as a co-vulcanization crosslinking agent for butyl gum and PVC glue, and can also be used alone as a crosslinking agent for PVC phenolic resin and the like. Dosage is generally about 1 part, and with Water treatment heavy metal ion capture agent copper flotation agent |